dc.identifier.citationCizek, J., & Khor, K. A. (2012). Role of in-flight temperature and velocity of powder particles on plasma sprayed hydroxyapatite coating characteristics. Surface and Coatings Technology, 206(8-9), 2181-2191.en_US
dc.identifier.issn0257-8972en_US
dc.identifier.urihttp://hdl.handle.net/10220/10331
dc.description.abstractThis paper presents a systematic research on the process of thermal spraying of HA encompassing all stages of layer deposition: powder production and characterization (optimized production led to spherical 39.90 ± 10.61 μm powder with 0.0% content of tri-calcium phosphate [TCP] or tetra-calcium phosphate [TTCP] phases), plasma jet properties influence on the in-flight powder properties (major influence of spray distance factor), the influence of the in-flight temperature and velocity of hydroxyapatite powder particles (ranges of 2294 K–2708 K and 152 m·s−1–291 m·s−1) on the final characteristics of the deposited coatings. Six combinations of the system parameters leading the low-medium-high in-flight properties were selected and the respective coatings were investigated, with some data in contradiction to previously published results. It was found that the temperature of the particles plays a critical role for the development of detrimental CaO (content increase of up to 14.6%) and metastable TTCP (up to 49.5%) phases in the coatings. Particle in-flight velocity was found to influence the open porosity of the coatings (8.8%–27.9%) and has an impact on the micro-hardness and moduli of the coatings (relative differences of up to 2.8×). Joint incidence of both in-flight properties was found to significantly influence the microstructure of the coatings and its respective surface roughness levels (Ra = 7.4–19.4 μm). The morphology of impinging splats was found to be influenced by both the in-flight velocity (dominant factor) and temperature (secondary factor) of the HA particles.en_US
dc.language.isoenen_US
dc.relation.ispartofseriesSurface and coatings technologyen_US
dc.rights© 2011 Elsevier B.V.en_US
dc.titleRole of in-flight temperature and velocity of powder particles on plasma sprayed hydroxyapatite coating characteristicsen_US
dc.typeJournal Article
dc.contributor.schoolSchool of Mechanical and Aerospace Engineeringen_US
dc.identifier.doihttp://dx.doi.org/10.1016/j.surfcoat.2011.09.058