dc.contributor.authorBadica, Petre
dc.contributor.authorGrasso, Salvatore
dc.contributor.authorBorodianska, Hanna
dc.contributor.authorXie, Sky Shumao
dc.contributor.authorLi, Peifeng
dc.contributor.authorTatarko, Peter
dc.contributor.authorReece, Mike J.
dc.contributor.authorSakka, Yoshio
dc.contributor.authorVasylkiv, Oleg
dc.date.accessioned2014-09-11T07:37:24Z
dc.date.available2014-09-11T07:37:24Z
dc.date.copyright2014en_US
dc.date.issued2014
dc.identifier.citationBadica, P., Grasso, S., Borodianska, H., Xie, S. S., Li, P., Tatarko, P., et al. (2014). Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600^|^deg;C) spark plasma sintering. Journal of the Ceramic Society of Japan, 122(1424), 271-275.en_US
dc.identifier.issn0914-5400en_US
dc.identifier.urihttp://hdl.handle.net/10220/20506
dc.description.abstractDense boron carbide (above 95%) was achieved through high pressure (300 MPa) and low temperature (1600°C) Spark Plasma Sintering (SPS). This approach resulted in improvement of fracture toughness and of dynamic toughness when compared to corresponding toughness values of the sample sintered by conventional SPS (2100°C, 50 MPa). Dynamic toughness was extracted from Split Hopkinson Pressure Bar measurements. Results are understood based on microstructure and on very different behaviour of the samples in respect to residual B2O3 and carbon available in the raw B4C powder.en_US
dc.language.isoenen_US
dc.relation.ispartofseriesJournal of the ceramic society of Japanen_US
dc.rights© 2014 The Ceramic Society of Japan. This paper was published in Journal of the Ceramic Society of Japan and is made available as an electronic reprint (preprint) with permission of The Ceramic Society of Japan. The paper can be found at the following official DOI: http://dx.doi.org/10.2109/jcersj2.122.271.  One print or electronic copy may be made for personal use only. Systematic or multiple reproduction, distribution to multiple locations via electronic or other means, duplication of any material in this paper for a fee or for commercial purposes, or modification of the content of the paper is prohibited and is subject to penalties under law.en_US
dc.subjectDRNTU::Engineering::Materials::Ceramic materials
dc.titleTough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sinteringen_US
dc.typeJournal Article
dc.contributor.researchTemasek Laboratoriesen_US
dc.identifier.doihttp://dx.doi.org/10.2109/jcersj2.122.271
dc.description.versionPublished versionen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record