Please use this identifier to cite or link to this item:
https://hdl.handle.net/10356/142899
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Fu, Hua | en_US |
dc.contributor.author | Zhu, Wei | en_US |
dc.contributor.author | Xu, Zhongfeng | en_US |
dc.contributor.author | Chen, Peng | en_US |
dc.contributor.author | Yan, Chunze | en_US |
dc.contributor.author | Zhou, Kun | en_US |
dc.contributor.author | Shi, Yusheng | en_US |
dc.date.accessioned | 2020-07-07T06:57:39Z | - |
dc.date.available | 2020-07-07T06:57:39Z | - |
dc.date.issued | 2019 | - |
dc.identifier.citation | Fu, H., Zhu, W., Xu, Z., Chen, P., Yan, C., Zhou, K., & Shi, Y. (2019). Effect of silicon addition on the microstructure, mechanical and thermal properties of Cf/SiC composite prepared via selective laser sintering. Journal of Alloys and Compounds, 792, 1045-1053. doi:10.1016/j.jallcom.2019.04.129 | en_US |
dc.identifier.issn | 0925-8388 | en_US |
dc.identifier.uri | https://hdl.handle.net/10356/142899 | - |
dc.description.abstract | Carbon fiber reinforced silicon carbide (Cf/SiC) composite was fabricated by infiltrating liquid silicon (Si) into the carbon preform, which was built by selective laser sintering (SLS) additive manufacturing process from the phenolic resin coated carbon fiber powder with addition of submicron Si. The effect of Si addition on the microstructures of the laser-sintered green part, carbon preform and derived Cf/SiC composite was investigated. The results show that the introduced submicron Si plays an important role in reducing porosity and average pore size of the carbon preform, and contributes to improving the microstructure homogeneity of Cf/SiC composite by reducing the size of continuous bulk carbon in the preforms. The maximum density, flexural strength and fracture toughness of the Cf/SiC composite are 2.89 ± 0.01 g/cm3, 237 ± 9.6 MPa and 3.56 ± 0.24 MPa m1/2, respectively. The coefficient of thermal expansion (CTE) of the Cf/SiC composite is approximately 5.5 × 10−6/K from 25 to 900 °C, and the thermal conductivity is in the range of 74–84 W/m·K at room temperature, while decreases to 35–40 W/m·K at 900 °C. | en_US |
dc.language.iso | en | en_US |
dc.relation.ispartof | Journal of Alloys and Compunds | en_US |
dc.rights | © 2019 Elsevier B.V. All rights reserved. This paper was published in Journal of Alloys and Compunds and is made available with permission of Elsevier B.V. | en_US |
dc.subject | Engineering::Mechanical engineering | en_US |
dc.title | Effect of silicon addition on the microstructure, mechanical and thermal properties of Cf/SiC composite prepared via selective laser sintering | en_US |
dc.type | Journal Article | en |
dc.contributor.school | School of Mechanical and Aerospace Engineering | en_US |
dc.contributor.research | Singapore Centre for 3D Printing | en_US |
dc.identifier.doi | 10.1016/j.jallcom.2019.04.129 | - |
dc.description.version | Accepted version | en_US |
dc.identifier.volume | 792 | en_US |
dc.identifier.spage | 1045 | en_US |
dc.identifier.epage | 1053 | en_US |
dc.subject.keywords | Carbon Fiber Reinforced SiC Ceramics | en_US |
dc.subject.keywords | Additive Manufacturing | en_US |
item.grantfulltext | open | - |
item.fulltext | With Fulltext | - |
Appears in Collections: | MAE Journal Articles |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
Effect of silicon addition on the microstructure, mechanical and thermal properties ...pdf | 1.45 MB | Adobe PDF | ![]() View/Open |
SCOPUSTM
Citations
10
36
Updated on May 18, 2023
Web of ScienceTM
Citations
10
31
Updated on May 26, 2023
Page view(s)
310
Updated on May 29, 2023
Download(s) 50
93
Updated on May 29, 2023
Google ScholarTM
Check
Altmetric
Items in DR-NTU are protected by copyright, with all rights reserved, unless otherwise indicated.