Please use this identifier to cite or link to this item:
https://hdl.handle.net/10356/95387
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Chen, X. J. | en |
dc.contributor.author | Yu, L. G. | en |
dc.contributor.author | Khor, Khiam Aik | en |
dc.contributor.author | Sundararajan, G. | en |
dc.date.accessioned | 2012-09-11T03:58:45Z | en |
dc.date.accessioned | 2019-12-06T19:13:52Z | - |
dc.date.available | 2012-09-11T03:58:45Z | en |
dc.date.available | 2019-12-06T19:13:52Z | - |
dc.date.copyright | 2007 | en |
dc.date.issued | 2007 | en |
dc.identifier.citation | Chen, X. J., Yu, L. G., Khor, K. A., & Sundararajan, G. (2007). The effect of boron-pack refreshment on the boriding of mild steel by the spark plasma sintering (SPS) process. Surface and Coatings Technology, 202(13), 2830-2836. | en |
dc.identifier.issn | 02578972 | en |
dc.identifier.uri | https://hdl.handle.net/10356/95387 | - |
dc.description.abstract | Mild steel samples were borided with and without boron pack refreshment using the spark plasma sintering (SPS) process. Results show that the borided samples with boron pack refreshment developed a thicker boride layer compared to that without boron pack refreshment for the same boriding duration. When boriding duration is t < 120 min, the boriding growth in the samples borided with boron pack refreshment followed a parabolic growth pattern. In contrast, the boride growth in samples processed without boron-pack refreshment deviates from parabolic at t = 60 min. Computer simulation shows that the boron concentration change in the boriding media during the boriding process is an important factor affecting the composition and final thickness of the boride layer. | en |
dc.language.iso | en | en |
dc.relation.ispartofseries | Surface and coatings technology | en |
dc.rights | © 2007 Elsevier B.V. This is the author created version of a work that has been peer reviewed and accepted for publication by Surface and Coatings Technology, Elsevier B.V. It incorporates referee’s comments but changes resulting from the publishing process, such as copyediting, structural formatting, may not be reflected in this document. The published version is available at:DOI [http://dx.doi.org/10.1016/j.surfcoat.2007.10.016]. | en |
dc.subject | DRNTU::Engineering::Materials::Mechanical strength of materials | en |
dc.title | The effect of boron-pack refreshment on the boriding of mild steel by the spark plasma sintering (SPS) process | en |
dc.type | Journal Article | en |
dc.contributor.school | School of Mechanical and Aerospace Engineering | en |
dc.identifier.doi | 10.1016/j.surfcoat.2007.10.016 | en |
dc.description.version | Accepted version | en |
item.grantfulltext | open | - |
item.fulltext | With Fulltext | - |
Appears in Collections: | MAE Journal Articles |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
22. The Effect of Boron-Pack Refreshment on the Boriding.pdf | 690.54 kB | Adobe PDF | ![]() View/Open |
SCOPUSTM
Citations
20
11
Updated on Mar 20, 2023
Web of ScienceTM
Citations
20
10
Updated on Mar 24, 2023
Page view(s) 5
1,048
Updated on Mar 31, 2023
Download(s) 5
549
Updated on Mar 31, 2023
Google ScholarTM
Check
Altmetric
Items in DR-NTU are protected by copyright, with all rights reserved, unless otherwise indicated.