Please use this identifier to cite or link to this item: https://hdl.handle.net/10356/96585
Full metadata record
DC FieldValueLanguage
dc.contributor.authorBothe, Martinen
dc.contributor.authorMya, Khine Yien
dc.contributor.authorJie Lin, Esther Marieen
dc.contributor.authorYeo, Chee Chuanen
dc.contributor.authorLu, Xuehongen
dc.contributor.authorHe, Chaobinen
dc.contributor.authorPretsch, Thorstenen
dc.date.accessioned2013-06-13T06:38:17Zen
dc.date.accessioned2019-12-06T19:32:47Z-
dc.date.available2013-06-13T06:38:17Zen
dc.date.available2019-12-06T19:32:47Z-
dc.date.copyright2012en
dc.date.issued2012en
dc.identifier.citationBothe, M., Mya, K. Y., Jie Lin, E. M., Yeo, C. C., Lu, X., He, C., et al. (2012). Triple-shape properties of star-shaped POSS-polycaprolactone polyurethane networks. Soft Matter, 8(4), 965-972.en
dc.identifier.issn1744-683Xen
dc.identifier.urihttps://hdl.handle.net/10356/96585-
dc.identifier.urihttp://hdl.handle.net/10220/10344en
dc.description.abstractHere, we present an investigation of the triple-shape properties of star-shaped polyhedral oligomeric silsesquioxane-poly(ε-caprolactone) polyurethanes (SPOSS-PUs), which have three-dimensional network structures. In a typical ‘triple-shape functionalization process’, mostly consisting of two tensile deformations at different temperatures, chain immobilization of the polymer network component poly(ε-caprolactone) (PCL) was successfully realized first through crystallization and then through vitrification. Subsequently, large parts of the respective strains were released under stress-free recovery conditions. The two-fold fixed (‘programmed’) specimens responded to heating with two independent length contractions (switching steps); the first shape change was associated with PCL devitrification and the second one with the melting of hitherto crystalline PCL. It was revealed that the triple-shape properties of SPOSS-PU networks considerably depend on PCL network chain length. When applying exactly the same ‘triple-shape creation procedure’, larger strain releases were detected in the first transition for polymers with a higher PCL network chain length, whereas the second transition was more accentuated for SPOSS-PU networks with a shorter PCL chain length. In the course of thermo-mechanical cycling, the formation of a neck during the second tensile deformation was repeatedly detected for SPOSS-PUs with higher PCL network chain length; in the subsequent recovery process the specimens even exhibited the highest total strain recoverability. Finally, gradual strain release could be achieved at temperatures below the PCL melting transition through the selection of up to four temperature holding steps, at which every time stable shapes were formed.en
dc.language.isoenen
dc.relation.ispartofseriesSoft matteren
dc.rights© 2012 The Royal Society of Chemistry.en
dc.titleTriple-shape properties of star-shaped POSS-polycaprolactone polyurethane networksen
dc.typeJournal Articleen
dc.contributor.schoolSchool of Materials Science and Engineeringen
dc.identifier.doihttp://dx.doi.org/10.1039/c1sm06474fen
item.grantfulltextnone-
item.fulltextNo Fulltext-
Appears in Collections:MSE Journal Articles

Google ScholarTM

Check

Altmetric

Items in DR-NTU are protected by copyright, with all rights reserved, unless otherwise indicated.